PriceList for Sulfonated Lignite For Drilling - Fluid Loss Additives-OBC-G80L – Oilbayer

Short Description:


Product Detail

Related Video

Feedback (2)

As for aggressive costs, we believe that you will be searching far and wide for anything that can beat us. We can state with absolute certainty that for such high-quality at such rates we have been the lowest around for Drilling Fluids Additives , Cmc Oil Drilling Grade , Drilling Fluid Polyacrylamide Polymer , Presently, we are looking forward to even greater cooperation with overseas customers based on mutual benefits. Please feel free to contact us for more details.
PriceList for Sulfonated Lignite For Drilling - Fluid Loss Additives-OBC-G80L – Oilbayer Detail:

Summary

OBC-G80L is a kind of sulfonic fluid loss additive. It has characters like: anti high temperature, anti-salt, quick strength development, few free water. The product is appropriate to be used in different kinds of water and cement. It is also a kind of widespread use product, which can be used in different kinds of cement slurry systems. OBC-G80L is not only applicable in freshwater cement slurry, but also applicable in salt water cement slurry.

Functions

It decreases the fluid loss obviously. Generally less than 50ml.If increasing the dosage, fluid loss will less than 30ml.

Effective salt resistance. It can be used in saturated salt water.

Thickening time increases slightly as temperature increases in the temperature range of 70 to 90℃. It has no influence on the strength of cement stone.

Not sensitive to dosage, no catastrophe point, safety in use.

Usage range

Temperature: ≤180℃ (BHCT)

Recommend dosage:4.0~6.0% (BWOC)

Applicable in every kind of cement slurry systems, which are composed by every grade of oil-well cement(defined by GB10238 or APISpec10A) and other additives(just like silicon powder, drift beads, flyash, bentonite, barite powder and hematite).

Technical data

Item

Index

Appearance

Colorless or light yellow sticky liquid

Fluid loss(50℃,6.9MPa,30min),mL

≤50

Free water(50℃),mL

≤1

pour point, ℃ (winter)

≤-15

Composition of cement slurry: SD“G”cement 800g, fresh water 340g, OBC-G80L 32g,  OBC-X60L 4g.

Packing

50L/plastic drum, or 200L/plastic drum. Or based on customers' request.

Storage

It should be stored in cool, dry and ventilated areas and avoid being exposed to the sun and rain.

Shelf life:24 months.

 


Product detail pictures:

PriceList for Sulfonated Lignite For Drilling -
 Fluid Loss Additives-OBC-G80L – Oilbayer detail pictures


Related Product Guide:
You did it! Toxic chemical banned in EU textile imports | Well Cementation Fluids In Oil Field
Global 9-decanoic acid methyl esterMarket 2018 Key Players, Share, Industry Key Drivers | Defoamer For Oil Well Cementing

Innovation, excellent and reliability are the core values of our firm. These principles today more than ever form the basis of our success as an internationally active mid-size corporation for PriceList for Sulfonated Lignite For Drilling - Fluid Loss Additives-OBC-G80L – Oilbayer, The product will supply to all over the world, such as: Mali , Netherlands , Sydney , With good quality, reasonable price and sincere service, we enjoy a good reputation. Products are exported to South America, Australia, Southeast Asia and so on. Warmly welcome customers at home and abroad to cooperate with us for the brilliant future.
  • This is the first business after our company establish, products and services are very satisfying, we have a good start, we hope to cooperate continuous in the future!
    5 Stars By Amy from Zurich - 2016.08.21 14:13
    Customer service staff and sales man are very patience and they all good at English, product's arrival is also very timely, a good supplier.
    5 Stars By Emma from Algeria - 2015.06.18 17:25
    
    WhatsApp Online Chat !