To become the stage of realizing dreams of our employees! To build a happier, much more united and far more professional team! To reach a mutual profit of our clients, suppliers, the society and ourselves for Fluid Loss Additive , Wellbore Strengthening Materials , Oil-Base/Synthetic-Base Drilling Fluid Additive , Standing still today and searching into the long run, we sincerely welcome shoppers all around the globe to cooperate with us.
Discount Price saturation Salt Dispersant - Fluid Loss Additives-OBC-G80L – Oilbayer Detail:

Summary

OBC-G80L is a kind of sulfonic fluid loss additive. It has characters like: anti high temperature, anti-salt, quick strength development, few free water. The product is appropriate to be used in different kinds of water and cement. It is also a kind of widespread use product, which can be used in different kinds of cement slurry systems. OBC-G80L is not only applicable in freshwater cement slurry, but also applicable in salt water cement slurry.

Functions

It decreases the fluid loss obviously. Generally less than 50ml.If increasing the dosage, fluid loss will less than 30ml.

Effective salt resistance. It can be used in saturated salt water.

Thickening time increases slightly as temperature increases in the temperature range of 70 to 90℃. It has no influence on the strength of cement stone.

Not sensitive to dosage, no catastrophe point, safety in use.

Usage range

Temperature: ≤180℃ (BHCT)

Recommend dosage:4.0~6.0% (BWOC)

Applicable in every kind of cement slurry systems, which are composed by every grade of oil-well cement(defined by GB10238 or APISpec10A) and other additives(just like silicon powder, drift beads, flyash, bentonite, barite powder and hematite).

Technical data

Item

Index

Appearance

Colorless or light yellow sticky liquid

Fluid loss(50℃,6.9MPa,30min),mL

≤50

Free water(50℃),mL

≤1

pour point, ℃ (winter)

≤-15

Composition of cement slurry: SD“G”cement 800g, fresh water 340g, OBC-G80L 32g,  OBC-X60L 4g.

Packing

50L/plastic drum, or 200L/plastic drum. Or based on customers' request.

Storage

It should be stored in cool, dry and ventilated areas and avoid being exposed to the sun and rain.

Shelf life:24 months.

 


Product detail pictures:

Discount Price saturation Salt Dispersant -
 Fluid Loss Additives-OBC-G80L – Oilbayer detail pictures


Related Product Guide:
EPA adds NPEs to Toxics Release Inventory | 2018-06-25 | Defoamer For Oil Well Cementing
OTCMKTS:HCGS | Well Cementation Fluids In Oil Field

abide by the contract", conforms on the market requirement, joins from the market competition by its good quality likewise as provides more comprehensive and superb support for customers to let them become large winner. The pursue of the company, is definitely the clients' pleasure for Discount Price saturation Salt Dispersant - Fluid Loss Additives-OBC-G80L – Oilbayer, The product will supply to all over the world, such as: Auckland , Swaziland , California , The president and all the company members would like to provide qualified goods and services for customers and sincerely welcome and cooperate with all native and foreign customers for a bright future.
  • The accounts manager made a detailed introduction about the product, so that we have a comprehensive understanding of the product, and ultimately we decided to cooperate.
    5 Stars By Christian from British - 2016.06.19 13:51
    Managers are visionary, they have the idea of "mutual benefits, continuous improvement and innovation", we have a pleasant conversation and Cooperation.
    5 Stars By Beatrice from Peru - 2015.09.21 11:01
    
    WhatsApp Online Chat !